my attemts at lip-sync were hindered by hot lights and melting plastercine which became very shiny. my original plan was to replace pre made mouth parts as different sounds are created, this was impossible due to the sticky plastercine losing its original shape. the results are very rough , next step is to recreate the whole face and seperate jaw using fimo. plastercine can be used to smooth out the join but thats all. Moving the armature itself was a bit better but I still need lots of practice before anything descent will happen.